Specification:
Composition :Epoxy acrylate oligomer & acrylate monomer
Viscosity(cps/25℃):190 ± 20
Appearance:Light yellow liquid
Solvent :-----
Solid content(%) :99
Odor :Light amine
End Use:
Varnish for thin paper board
Application & Test:
Process:
CH-70114 =>Print machine coater roller coating
=>UV curing(80watt/cm High-pressure mercury vapor lamp or metal-halide lamp)
Film Special property:
(1)Good leveling and gloss
(2)High hardness
(3)Instant cure
(4)Abrasion resistance and chemical resistance
(5)Superior adhesion
(6)Non-yellowing
FAQ
1.Q: Are you a factory or trading company?
A: Yes, we are one of the most professional manufacturers for overprinting varnish for printed paper substrates, includes different products line, Water based resin ,Solvent based resin, UV resin.
2.Q: How can I get some samples?
A: We are honored to offer you samples by express.
3 Q: How does your factory do regarding quality control?
A: Quality is the priority. We always pay much attention to quality control from beginning to end.
-----------------------------------------------------------------------
General questions for Water based resin
Q1: Why we can find the “White point” on surface ?
A: There are too many factors have lead to fail mirror surface , such as the paper too rough , varnish too thin , varnishing speed too high, too many powders when it printing , roller’s rubber too old to use…etc.
Solution: Please build the varnish up , slow down the speed and change the new rubber for operate more smoothly.
Q2 : Why not gloss after varnishing ?
A: Please raise up the temperature for iron board (more than 100 degree ) and pressure more than 125KG/CM2 , add up more varnish or change iron board for improving.
Q3: Blocking paper
A: Please keep down the temperature and slow down the varnishing speed to improve volatility too fast.
Q4: Why Ink spread out after varnishing ?
A: You can varnishing after confirm the ink already dry , change the solvent or keep down the pressure of varnishing machine.